Ring tutorial

Started by mizgeorge, January 21, 2009, 02:34:23 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Chameleon

It was lots of fun, and much easier than i thought thanks to the great instructions  ;)

Margram

Quote... and what can I use instead of a ring mandrel....?? 
I read somewhere that you can use a thick magic marker pen barrel, and if it is too small put some layers of masking tape on top.

Marg x
Marg x  Etsy Flickr My blog

Blue Kiln Beads

Thanks for the tut George, very generous of you to take the time to do the instructions.
Yvette Goodridge
www.bluekilnbeads.blogspot.com
www.bluekilnbeads.etsy.com

mizgeorge


lorrainelee

I've never tried wire wrapping before and I  only had my phone handy to take a piccie, but, this is one of my beads with the George's tutorial and, I'm chuffed to bits with it  (even though it's very very amateurish and a cr..p picture!!)


Thank you George!! :-* :-*
Lorraine

fionaess

Quote from: Margram on January 22, 2009, 12:50:06 PM
Quote... and what can I use instead of a ring mandrel....?? 
I read somewhere that you can use a thick magic marker pen barrel, and if it is too small put some layers of masking tape on top.

Marg x
Thanks Marg... I made one using copper wire and its far too small... but this is the first wire tutorial that I have actually been able to understand and 'do' fairly competently... Thanks George :) :)


If it's got a hole, it's a bead !

Lloki

Brilliant!
If this is just a rough version, I'd love to see a polished one!
Thank you for sharing with us!
Cerri

mizgeorge

Lorraine - that's fab!

I'm so pleased that people are having a go!

You may be seeing more tutorials from me in months to come ;)

julieHB

Quote from: mizgeorge on January 22, 2009, 07:41:41 PM

You may be seeing more tutorials from me in months to come ;)

I for one would look forward to that a lot!!  ;D
Julie xx

                           My Webbie - My Flickr

Funky Cow

Thanks for sharing that George  :-*
Cathryn xxx     


My Etsy: http://funkycow.etsy.com

lorrainelee

Quote from: julieHB on January 22, 2009, 07:51:32 PM
Quote from: mizgeorge on January 22, 2009, 07:41:41 PM

You may be seeing more tutorials from me in months to come ;)

I for one would look forward to that a lot!!  ;D
I would too - pretty please.
Lorraine

turnedlight

Here you are, my first was the one on the left, it's very wonky, but the others are better! I made some flatter beads for the purpose of doing the rings. I really enjoyed it, except my thumb is really sore! I guess that's what comes of not doing silver work for a while..
Thank you so much for the tut!
 
       

;D
kathryn

fionaess

Those are lovely Kathryn  ;D ;D


If it's got a hole, it's a bead !

mizgeorge

Love 'em! Especially the orange one :)

kevie192

Ooooh, these are beautiful!! Thanks for the tut, George!

Must get some beadies and wire and give it a go! Anyone sell singles? :D

Kevin x