Started by Rachel B, June 01, 2008, 10:28:57 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Rachel B

I really love them and want to have a go at making some, is it just a case of clear frit not melted in or is it more complicated?  I can remember seeing a set that Anna Beads on Toast made ages ago called coconut ice, Anna, want to share your secret??  Thanks all.

Billie

On a Canadian forum, someone had posted similar with a pink base and gold frit... Blimey they looked gorgeous!!  It was the Two Glassy Ladies site  ;D

beads-on-toast

clear frit

and that's it

i am a poet

and i did not know it ha ha

Yup crystal cleat frit, (beady sam has it) called Lead i think

Watch it doesn't go sooty and use it high in the flame

x x x

Rachel B

Cheers Anna, I shall add that to my shopping list (It`s over a mile long ya know!) thanks for sharing. :)

Clare Scott

You will need some k100 lead crystal frit - its really fine x