Main Menu

Using COE 90 frit with 104

Started by ShinySnail, June 15, 2011, 01:40:06 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

ShinySnail

Hiya,
I have been busy making a few BHB sets to sell on a friends stall at a fair this Sunday, and haven't had too much reservation before about using COE 90 frit with 104 glass.... until I had a breakage yesterday

Now I'm having a mini freak out as these are going to be the first things I have ever made for sale!

In other peoples experience, am I taking a risk? I have been making some pretty substantial doughnuts with a layer of the frit encased and a layer on top (it's really fine frit)

Any comments or opinions would be greatfully received. I spent an entire day making these in different colour combinations so it would be a real gutter to condem them to the fugly jar - but i'd much prefer to do that if it means I don't dissappoint people and ruin my credibility  :-\

Thanks,
Anna

Kaz

My own view would be that 90 is too far away from 104. I happily use 94/96 with 104 and have generally had no problems. If you want to use 90 COE frit, why not get some bullseye to work with?
In any case I would leave these a while before selling just in case they do develop problems. I did have problems with one set last year that I had made in Oz and brought back for annealing but have had no other problems with using 104 with 94/96. I've never tried anything lower other than with bullseye.
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

ShinySnail

Thanks Kaz, I had a feeling that would be the answer  ;)
Just glad I had the break now rather than later as that's what prompted me to investigate...

nooooooo all that time wasted!

awrylemming

Commiserations hun - but it could have been worse, you might have sold them!  :o  There's still time to make more xx

ShinySnail

Yeah I know thanks Sue  :)
Bad times though! And this news came at the same time as the discontinued CIM colours too OMG