helenfc

 :o thats gorgeous fiona didnt know siver brown was capable of that!! :)

Trudi


fionaess

Thanks - they are silver brown on cobalt transparent and then encased...


If it's got a hole, it's a bead !

silverlemon

Bionic Sarah xxx    Sarah Downton On Facebook  My Etsy Shop

kerensky

Quote from: fionaess on March 25, 2010, 07:48:51 PM
Thanks - they are silver brown on cobalt transparent and then encased...

Wow - and they are also Gorgeous!


Clair

Blimey! Well, that's me off to the old garage to practice some more. They are stunning - the reactions are amazing!

fionaess

You don't see the colour until you encase.. so don't keep reducing while muttering to yourself,,,, she said they would go blue when I reduced, where is the bloody blue.. I hate this glass, it must be my torch, set up, crap batch of glass, wind in the wrong direction or that damn woman didn't tell me how to do it right  ;D ;D ;D ;D


If it's got a hole, it's a bead !

Ilona


♥♥Tan♥♥

Gorgeous Fiona you clever thing!

Clair

Quote from: fionaess on March 27, 2010, 05:36:04 PM
You don't see the colour until you encase.. so don't keep reducing while muttering to yourself,,,, she said they would go blue when I reduced, where is the bloody blue.. I hate this glass, it must be my torch, set up, crap batch of glass, wind in the wrong direction or that damn woman didn't tell me how to do it right  ;D ;D ;D ;D