Started by bbbeads, August 01, 2016, 03:11:49 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

bbbeads

Can anyone tell me if the bead door when closed is completely sealed or is there a gap left round the edges.  Thinking of buying a door for my paragon SC2 but I want to use it still for enamelling.   I know there will be a gap when putting mandrels in to garage the bead.

Trudi

You will probably find that it's not as sealed as a proper closed door. When I want to fuse in mne I have a piece of fibre blanket cut to fit inside the slot to help keep the heat in. Seems to work for that purpose. Hope that helps!

bbbeads

Thank you for information I will do that when enamelling.

fionaess

I have an SC3 with a bead door that I use for annealing and enamelling.  I just leave the bead door shut and keep an eye on the controller temp when I enamel.. You lose far more heat opening the main door than the tiny amount through the closed bead door :)


If it's got a hole, it's a bead !

flame n fuse

my paragon has a clip to keep the door shut. Never had a problem with fusing in it.