Started by beadammed, November 08, 2015, 07:58:02 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

beadammed

Anyone used colours de verre moulds with bullseye frit? I have the lily pad and frog Mould I am about to try out in my hobby fuser and would appreciate any advice on programs. Thanks
Geraldine
www.etsy.com/uk/shop/strikingglassstudios

JKC

I have used a few of them.  They have advice for all of them on their websites.  I use boron spray instead of kiln wash.  Janet

beadammed

Thanks Janet. l'll give it a go
Geraldine
www.etsy.com/uk/shop/strikingglassstudios

beadammed

I followed the recommended schedule and it fused perfectly. I'm currently slumping it ;D
Geraldine
www.etsy.com/uk/shop/strikingglassstudios

flame n fuse

sounds good, looking forward to the photos!

beadammed

Geraldine
www.etsy.com/uk/shop/strikingglassstudios

Mars


Moira HFG

Oh, very nice. You've got a lovely smooth edge on that leaf.

Glassy Lou


beadammed

Thanks, I was happy with my first attempt.  Would put less glass in the wee frog tho.
Geraldine
www.etsy.com/uk/shop/strikingglassstudios

JKC

Very nice, glad they came out well.  I have just had to make a few adjustments here and there, the schedules are very good.  Janet