Author Topic: Quick Question - fill weight on small mosaic mould  (Read 1291 times)
0 Members and 1 Guest are viewing this topic.
Mars
Forum Member
*
Posts: 36


« on: March 01, 2016, 12:27:40 PM »

Hello!

Just a quickie, does anyone know the fill weight for the squares in this mould?

http://www.warm-glass.co.uk/foursquare-mosaic-mould-8001-p-1215.html?cPath=96_152

It's the Four-Square small mosaic mould, I've done a quick search and I know I can experiment, but wondered if anyone else was using this one?

In the other casting moulds I've got they give guides but can't find anything for this one other than heap up the frit in a mound Smiley

Cheers!
Mars xx
Logged
smudges dad
New Forum Member
*
Posts: 15


« Reply #1 on: March 01, 2016, 12:56:25 PM »

Easiest way is to find the volume of water in ml, then multiply by 2.5 to get grams
Logged
Mars
Forum Member
*
Posts: 36


« Reply #2 on: March 01, 2016, 03:24:29 PM »

Ooh thanks, I didn't know that!