Main Menu

LIQUID STRINGER PART 2

Started by DeePoole, September 08, 2014, 08:12:11 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

DeePoole

This is just a short one to show how the lace tree was finished, and liquid stringer directly onto sheet and coloured in. Nice and easy! If I can do it, a banana could do it!
http://www.youtube.com/watch?v=Jo2mUnqmnwo

Margram

Marg x  Etsy Flickr My blog

Pat from Canvey

You could also use Gum Tragacanth from Hobbycraft instead of the Tylo powder.

Opalshards

Just been looking around your site Dee.
You do some amazing work. I especially like your mermaids.

DeePoole

It's true, you can use many things to make the gel. This is what works for me, but it isn't the only product that does the same.
As long as we make it rather than spending a lot buying it..x

shafeenan

Probably obvious to the rest of you, but to save having too many colours in stock, can one successfully mix powdered frit to get extra colours or do they separate?
thanks