Pat from Canvey

One thing I don't think others have mentioned is that you should keep a firing log. Record what glass, timing, what program, whether fuse, slump etc and the results so that you can replicate in future. It's also important to record failures for whatever reason so that you can avoid them in future.

Barnacle Bay

Quote from: Pat from Canvey on March 12, 2014, 03:34:29 PM
One thing I don't think others have mentioned is that you should keep a firing log. Record what glass, timing, what program, whether fuse, slump etc and the results so that you can replicate in future. It's also important to record failures for whatever reason so that you can avoid them in future.