Main Menu

Cool Kiwi

Started by Glassy Lou, March 04, 2013, 01:47:10 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Glassy Lou

So far I've only managed to get a transparent dark green from this - no lovely streaks like I've seen on the sample pics. Do I have to do something special with it?
Any help would be greatly appreciated before I waste it all! :/

Louise x

justjules

I'm sure someone will come along with a better answer but I love cool Kiwi because I always get lovely streaks without doing anything technical, just splodge it on & hey presto (just wish it was cheaper!)

:)

Shirley

I just use it. Nothing special, although I do tend to work on the cool side with the propane turned down.

If you've been making small beads perhaps try making something a little bigger.
Val Cox Frit - Thai and Bali Silver 

Rascal

Hi, sorry I don't do anything special with it but have found some rods within a batch behave differently and some seem to be really dark almost transparent green with a few stripes and others are like the photos on the website. I've also found size of bead does vary, the smaller the bead the less the effect. Good luck.