So I have finally had time to read through Feb's issue of SDL. And love the article on size 0 frit. I have emailed Shirley to see if she has any val cox frit in size 0 in stock but can I get some from anywhere else? I prefer blends but I'm not fussy at the moment :) Thanks xx
Sarah xx
Website. Blog. Flickr.

♥♥Tan♥♥

I'm sure beadybugs does it. Is beadybugs right???

♥♥Tan♥♥


Shirley

#3
Just sent you an email, Sarah.

For anyone else, I have Raku Jitterbug, Fuchsia Pink, Winter Blues, Purple Rose and Dark Iris Gold in #0.

I should have some more for Flame Off as there are around 20 on the VC site now. Need to to get my order in fairly soon :)
Val Cox Frit - Thai and Bali Silver 

julieHB

And Kaz has some lovely K0 blends in her etsy shop:

http://www.etsy.com/shop/kazkebab
Julie xx

                           My Webbie - My Flickr

anditsinthefish

you guys are so helpful and so quick :) Thanks just going to do order of val cox until I can decided what else to order... to much to choose from! xx
Sarah xx
Website. Blog. Flickr.

Pat from Canvey

Shirley, are Fyrebirds going to be at the Essex Bead Fair on 24th Feb? I can't see your name on the current list of exhibitors.

Shirley

I'm going to be there as Shirley Giles, Pat. It was a bit of a last minute decision. I'll be bringing all the frit with with me so you should be able to have a good browse :)
Val Cox Frit - Thai and Bali Silver 

arachnia

Sarah I do size 0 frit too in 104coe if you are interested some of the frit is on sale too.
Vickie
]

james M knox

Hi All,

can someone enlighten me please - How big is size #0 and where can I find out the other sizes as well please

James

Lynnybobs

Size 0 is the fine stuff but I don't know the actual size range of the pieces
Lynnybobs
----x----

james M knox

Thanks for the Info

James

Beadbug

I have got some size 0 coming in very soon, hopefully by the end of the week. I am starting with a few colours and will then build up the stock of size 0.

There are some nice pinks in size 0 coming.

Kaz

Generally, size 0 is like caster sugar where size 1 is more like granulated sugar!
Kazx