Just wondered if anyone can reccommend a nice sparkly frit that I can add to clear glass for some christmassy beads, dont mind if its silver, gold or even read just as long as i get  a bit of a sparkle with it :)


ARBeads

Another way is to get some dicro, encase and pull stringers.

Ruth & Andy


www.etsy.com/shop/arjewellery for beads!

SilverGems89

or try pixie dust for a really good surface sparkle  ;)

Skyblue

Thankyou all very much :)) will look at all those options , I love this forums , you get such good advice.

ARBeads

Oh I'd forgotten about pixie dust, makes everything look sparkly including your extract - pretty.
Ruth & Andy


www.etsy.com/shop/arjewellery for beads!

Kaz

Or use silver foil melted in and then frit on top - avoiding any with pink, red or orange in them.
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Skyblue


tish

Quote from: Kaz on September 20, 2012, 10:28:58 PM
Or use silver foil melted in and then frit on top - avoiding any with pink, red or orange in them.
Kazx
why?

Trudi

Because of the way they react with silver,  you'll get a sludge colour!

The Tartan Trout

Quote from: Trudi on September 21, 2012, 08:02:33 AM
Because of the way they react with silver,  you'll get a sludge colour!

I was very good at making sludge beads a while back :)