I met a lady at a show yesterday who admired this bead:



She asked me to make her one similar in shades of pink or purple but with still with the surface reduction.  HELP!  I can get some great purples out of Kalypso but they are all encased.  I would be grateful for any ideas before I spend a fortune in glass to recreate a £15 pendant!  (I think this one was triton)

Carrie xx
www.CarrieandCo.folksy.com
www.carriehartshorn.etsy.com


Kalorlo

#1
Aurae's worth a try: can get it to go pinky-gold - might need multiple reduction cycles. You could try kalypso on the surface anyway and see what happens? Psyche gives dark purple/blue - try a light base for it?

Trudi

I Haven't played with Aurea for a while, and it can go pinky .. just can't remember how I did it.

Try a small test bead and try reducing while it's cold and another when it's still warmish.

You could even possibly try helios with a pink encased base?

CarrieH

I thought of helios but the lady was adamant that she 'didn't do golds'!  I also showed her some aurae over clear and this was too gold.  May have to try aurae over other colours and see what I can get.  My dayghter is home sick today so I've already lost a day when I could have been experimenting! :(

Carrie x
www.CarrieandCo.folksy.com
www.carriehartshorn.etsy.com


Lakelady

Boreas - the new DH one is more purple than Aurae, in a silvery kind of way  ;D
Turner Rowe Glass Art

spexy

Try Aurae over dark ivory.


ivory_aurae_bead by Earthshine Lampwork Bead and Jewellery Design, on Flickr

The flowers were encased with lavender 081 but you could try it without.

GaysieMay

Effetre silver purple reduces to give a lovely rich sheen :)
www.GaysieMay.etsy.com
www.facebook.com/gaysiemay

CarrieH

Do you mean the silver plum Gay? - I'd forgotten all about that!  I've only got the dark but it's worth a go.  Looks like I may get some torch time tomorrow as DD is desperate to go back to school for a school trip tomorrow.

Carrie x