Christmas Baubles - how?

Started by Ciel, April 13, 2012, 03:42:53 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

artbying

#30
Sorry Krysia@No98 I've found the info on how to post photos! so here goes

Bauble_-_Purple___Gold_Hedgehog by auraartglass, on Flickr
This was my first that sold in 2009

Krysia@No98



Oh WOW!!!  That's fabulous.  How big is it?

I've started with some blown hollows this week.  Baubles next...
-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

artbying

#32
Most of my baubles with silver rich glass generally measure 2.5 inch -3 inch diameter (approx 7cm) Height approx 3- 3.5 inch. (This is approx without getting one out to measure)  I have done larger, but this size are most controllable if using silver rich, striking or adding further decorations. I think I used Double Helix Psyche and Effetre EDF for the dots.  :)
Good luck with your baubles let me know if you need any help and I'll gladly do my best.

Lotti

Quote from: Ciel on April 20, 2012, 07:37:20 PM
I've just ordered the tutorial, so can't wait to received it and then have a play to see where I'm going wrong.

Hi, how did you get on with this Ciel, any piccies? :) :)