Clear glass

Started by liquidglass, August 05, 2012, 11:35:55 AM

Previous topic - Next topic

0 Members and 3 Guests are viewing this topic.

liquidglass

My clear glass turned into a smoky grey, have I got it too hot?
>:(

Dragonfire Glass

Possibly, but more likely too much propane in the flame, or melting too close to the yellow candles  :)

Magpie

Or running low on gas.