tish

i got some luna 2.1 from DH and to be honest im not acheiving much out of it ive tried striking and reducing and both together lol ive left plain and encased wish id bought clio now

Trudi

This one is just a striker (doesn't reduce) - have you tried encasing it?

tish


tish

ok i tried stricking and encaseing today anybody want to do a swap for whats left of the luna 2.1

Trudi

Did you make both on the same mandrel?

tish

no i just popped one on the end of the other for the piccy

tish

ok i will hold on to it unless anyones got any tangerine sparkle or clio