Main Menu

gallery archive 12

Started by Madam Steph, January 01, 2012, 12:41:00 PM

Previous topic - Next topic

0 Members and 5 Guests are viewing this topic.

moon44

Many thanks for those kind words.

Some flowers in the same colors as my hollows.
Hope you like them.



Monique.
Monique

mohennah-alamoon.blogspot.com
www.mohennah.com
http://www.facebook.com/profile.php?id=100000029877376http://
www.flickr.com/photos/41615533@N07/
http://www.etsy.com/people/Mohennah

binty

I had a first try at ring toppers, I think I'm addicted!


Untitled by binty13, on Flickr

Purple Cobwebs

Woooo, Helen, your ring toppers are fab. If they are your first, I can't wait to see where you go next with them!
Manuela, your heart just makes me feel happy and summery!
Helen V, what perfect dotty hearts. I dream of consistent dots!!!!
Spexy, what kind offerings for the swap, they are stunning.
Julia, what a lovely riot of colour!
Monique, I always gaze in awe at your amazing hollows and flowers!
Helen again, I love those colours! Very summery.
Ooh Jennie, what a gorgeous topper. It's almost ethereal!
Lisa, they are all fab. I love the one with te black squiggles....reminds me of a web.

I have been playing with new glass, new bead rollers, and new techniques (that still need to be worked on lots!)

First, my new favourite glass - Earth


Then Cool Kiwi with my new ornate bead roller


Then practising stringers after my class. Not brilliant but I like the resulting bead.


And then a bit of fun with my new brass frit! The centre bead is humongous as I was a bit enthusiastic with the frit so I had to keep encasing over and over to seal it in!!!

Gaynor
Making beads, cards and jewellery to raise funds for Viva and Dr Hadwens Trust!
www.purplecobwebs.co.uk

Jay9

I have been playing with new glass, new bead rollers, and new techniques (that still need to be worked on lots!)

First, my new favourite glass - Earth


No fair!  I stood there for ages trying to decide whether to buy some Earth and didn't bother.   Wish I had now. :(
Janine  xx

"You only retire when you stop doing something you don't like and start doing something you do"

lampworklover

Woa, I really wish I had bought earth now! Must put it on my birthday wish list.

Thought it was about time I showed something in here, must be a couple of hundred years since I last did so (when there was still a newbie show and tell  ;D). I have been playing with frit, as per...

Sin

Helbels - great ring toppers!  
Manuela - cheerful colours!
HelenV, Spexy - lovely beads!
Julia - cute dots!
Jennie - I admire your swirl beads, they are great!
Purple Cobwebs - the Earth beads are amazing!

I am currently proud of this bead:


mel

Great avatar Special Kay!

The FO has replaced my mojo with an alien's:
Before FO

Hadesanddots by melanie.ingledew, on Flickr

And after learning to work cool and slow with Manda, this arrived in the kiln this morning. A bit spooky, but I'm pleased with it technically!


spookyeye1 by melanie.ingledew, on Flickr
Laughinglass Lampwork Beads

Amber

It's fantastic to see how everyone has been inspired by the Flame Off, there is some amazing work here!

I haven't had a chance to play with my new toys yet, but here are a couple of beads made with black and white frit that I bought from Christina at last year's FO;




Blue Kiln Beads

Amber those beads are lovely, the top one reminds of granite. 

I've actually got something to show!  I have used some of awrylemming's lovely rainbow murrini  ;D  Some more pics on my blog.


Progress 001 by Blue Kiln Beads, on Flickr
Yvette Goodridge
www.bluekilnbeads.blogspot.com
www.bluekilnbeads.etsy.com

moon44

Love the rainbow murrini's in those beads.
Melanie your eye is great and spooky ;D

Summer from me:



Monique.
Monique

mohennah-alamoon.blogspot.com
www.mohennah.com
http://www.facebook.com/profile.php?id=100000029877376http://
www.flickr.com/photos/41615533@N07/
http://www.etsy.com/people/Mohennah

Magpie

Wow, that eye is amaxing! So's the dotty bead as well.
And the flowers and the rainbow beads......

I've been watching TV too much recently, I think.

????? by HelenPetersBeads, on Flickr
And I appear to be colour blind, DD took one look at him and said he's meant to be orange. All I saw was brown.

Ciel

Love that eye bead and the weird advert creature!

I've been busy making cats :)



HelenV

Just a few more from me this week:



Trying to get my stringer a bit better:



This one was with CIM Pimento that Sue very kindly sent me - its such a lovely orange:





Helen x

www.helenvanekdesign.co.uk
www.etsy.com/shop/helenvanekdesign

PeterG

I rather like the eye, it looks nice and evil.  What is the iris mad of?

I now have the celtic cross without the ring.  It's a little easier to make than the larger one although it still tends to shatter if you let one end get too cool.  It's a shame that the one on the right is stuck on the mandrel.



Peter

Josephine

So much here already. My favourites are those rainbow murrini beads and the two stripey cats.
A couple of sets from me.

sandytreasures4 by Josephine Wadman, on Flickr

pallida1 by Josephine Wadman, on Flickr