Brown glass?

Started by Mand, September 23, 2011, 04:09:15 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Mand

Hi again,

I have been making more and more brown coloured beads this autumn - I have plenty of dark, med and light amber, and dark brown bog standard poo coloured (sorry) effetre.  Are there any other minky-shade browns out there which are inexpensive? _ I'm thinking of etching which prob puts CIM Mink out of the picture?  Am just SO NOT a brown /green person as I usually like clear, bright colours ::)



Does anyone have any recommendations please?

Thanks.

Mand x

Les

Can't remember how well it etches ... bit CIM Stoneground is lovely .... and if you can still get it, Canyon de Chelly .... oh and Effetre red roof tile is lush :)

Les

This one's Stoneground ...


129_0066 by Mad Cat Glass, on Flickr

Mand

Mmm, yummy. Will give that ago, thanks. ;D  Any tips on a darker brown please?

Les

Didn't Effetre make a dark red or purply brown ?? Can't remember what the proper name was ...

Les

591452 Opaque Dark Brown Red

Mand


Les


Krysia@No98


have you looked at CiM Maple?

I am having the same problem.

Effetre seem to just do crayon chirpy brown and nothing more sophisticated.

(Would you like me to go through my colour chart this evening? )
-* -  Courage is going from failure to failure with out loosing enthusiasm -*-

paintboxcrafts

Cim maple is nice and it etches from what I remember.
www.paintboxcrafts.co.uk  www.paintboxcrafts.etsy.com

jammie

That's a lovely bead Les!  :) I've got some stoneground stashed.

Les

I adore stoneground .... it's very reactive with silver too :)

sarah t

for earthy browns i like sediment and mud slide

Madam Steph

One of my faves.. Lauscha Cocoa. 

It's good enough to drink  :)

ScarletLeonard

Quote from: Madam Steph on September 23, 2011, 07:20:38 PM
One of my faves.. Lauscha Cocoa. 

It's good enough to drink  :)

second that one.

or heat the snot out of CiM peace in a slightly reducing flame, it goes streaky brown then whack a thin layer of amber over it.