So this striking terracotta.

Started by ScarletLeonard, July 10, 2011, 04:18:24 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

ScarletLeonard

Striking it doesn't. Reducing, nada. All I have is how it looks on the rod - white.

awrylemming

Mine goes pinky coloured as I work it, the more it's in the flame, the pinker it goes.  But I'm on a minor, don't know about a hothead, but I would have thought it would be the same?

Fruddy

Scarlett - are you talking about Tongue Pink???

You need to let it reeeeallly cool and then reintroduce it.

Lotti

Infact, if you keep on doing it eventually it turns out burgundy, only happened to me once at one of Julie (Lush)'s courses and that was with a silver glass.  It does take some time to change and just when you think it is never going to happen it does.  I love it. :)

Lush!

Scarlet, just keep working it.  Like Rachel says, cool it then reheat and it will strike, it WILL strike.

It loves silver glass, and it loves silver foil or leaf too, honestly! Make a bead, roll it in a scrap of silver leaf, burnish it on, then back to the flame and heat all over.  :)


www.lushlampwork.etsy.com

ScarletLeonard

Thanks ladies.

I shall have another play with it tomorrow.
Just seemed to take forever to do nothing, it was nearly running off the mandrel I let it cool, gave it a roll in my bead roller, stuck it under the desk to check it was cool and wafted until I got bored.

I need to see all these lovely colours you keep mentioning Julie.

SilverGems89

Send me a rod or three and i'll test it for you Scarlet  ;) :P ;D

Dragonfire Glass


ScarletLeonard

Quote from: SilverGems89 on July 10, 2011, 07:19:30 PM
Send me a rod or three and i'll test it for you Scarlet  ;) :P ;D

How about NO! :p

theknittinggoddess

So glad it's not just me that can't get this to work...

Shirl

I have had a play with mine and I get a range of pale teracotta pinks out of it. If it put it back in the flame and get it too hot again it goes back to white! I have made one today and wrapped it in foil, then rolled it in my ribbed beadroller......hope it turns out ok when its cooled!

SilverGems89

Quote from: ScarletLeonard on July 10, 2011, 07:54:58 PM
Quote from: SilverGems89 on July 10, 2011, 07:19:30 PM
Send me a rod or three and i'll test it for you Scarlet  ;) :P ;D

How about NO! :p

Spoil sport! I need to sell something now so i can order glass and get some free  :P

Lush!

Right then, doubters  ;D

I made some beads, took some (pretty awful) pics and wrote some words - here you go  :D

http://juliefountain.blogspot.com/2011/07/striking-terracotta.html