awrylemming

Does this count Les?


first murrini by awrylemming, on Flickr

My first ever murrini  ;D  I feel like a proud mother  ::)
I used rubino, ocean and poi.

jammie


awrylemming

Want some?  I may be up to my ears in murrini before very long  :o  And I'm a little bit addicted ...

helenfc

Go Sue!! ;D
They are fantastic, glad to hear you are getting addicted,lol, you are going to need a few more of those wee murrini trays soon! xxx

jammie

Quote from: awrylemming on April 13, 2011, 06:25:57 PM
Want some?  I may be up to my ears in murrini before very long  :o  And I'm a little bit addicted ...

do bears pray and popes dump in the woods!!  ::) :-*

Shirl

Oh Sue...you clever thing you :) its fab!!!!!

The Tartan Trout


poledra1958

Some Poi with some of Kaz's "in the night" frit from the fire and ice set using one of my new presses got at FO.  (Also my third attempt at a cab which I am going to try to make into a ring)


HH on Bulk,

DellaUK

#23
Here's my offering:



Della

ebay: goodturnlampworkdella  web: www.goodturnlampwork.co.uk

Les

Quote from: awrylemming on April 13, 2011, 06:02:42 PM
Does this count Les?


first murrini by awrylemming, on Flickr

My first ever murrini  ;D  I feel like a proud mother  ::)
I used rubino, ocean and poi.

why of course ;D

Trudi

Ohh loving this - I bought some of this at FO as it's not a colour I've used!

Here's mine - made up into a bag charm!


Raffle Prize by Glittering Prize - Trudi, on Flickr

Beads by Jules

Scarlet,

You did bring Poi back from FO, problem was you brought it for me  :D

I've never tried one of these challenges, I will have to have a go this week!

Jules x

ScarletLeonard

Doh!

I have some now thanks to Marg. Totally forgot it was in the little bundle I bought you. Though if I had remembered it would have been gone before the glass got to you.

Ah well.

Got a few ideas I want to try now, if only there were more hours in the day.

flowerjasper

old beads, but a lovely reaction between poi and mystic green,

sandy

Magpie

Lovely reaction. It also reacts on top of bordello (i'm sure someone last month in the theme challenge said purples and reds react well) Here's poi flowers over bordello, very happily splitting, the 'vine cane' is just a poi stringer which has the lovely line down the middle, what a cheat! ;D

Flowery glass bhbs by HelenPetersBeads, on Flickr