Where's the element on a Beadcube?

Started by helbels, March 26, 2011, 06:41:16 AM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

helbels

Is the element in the Beadcube at the top or bottom?  I had better results with Terranova overnight, but some beads still struck more than others and I am guessing it may have been the ones nearest the element.

sarah t

i thought the side on the right with the dimps where i first put the beads was slighty hotter ....no idea where the element is ...thats one for lee or check out the site  that might tell you

Lee - Kilncare

O.K. then, the elements actually wraps all around the chamber of the bead cube.
It is one long element and when it is installed there is only a few milimeters between each wrap.

If you look carefully at the interior of the Cube you can sometimes make out the "ribs" that hold the element and it is then clear to see just how close the elements are.

With the elements being so close it effectively turns the whole of the floor, sides and roof a hot plate.

There is no heat in the rear wall or door.

TWITTER @kilncare
VISIT US ON FACEBOOK FOR THE LATEST ON US.
http://www.facebook.com/pages/Stoke-On-Trent-United-Kingdom/Kilncare-Ltd/238801689732

helbels

Thanks Lee - that's my theory blown out the water then!!!!  :D :D