julieHB

I cannot remember for the life of me who said it, but I am sure I have been told that, whichever bead release you use, it is important to keep the bead release warm for it to keep sticking to the mandrel and not breaking after it has initially been warmed up. This may be the reason why people have problems with cracking when using presses and when making long beads. Just a thought... :)
Julie xx

                           My Webbie - My Flickr

Veebee

Hmm, I do always get it straight back in the flame after pressing, but I will bear that in mind, thanks Julie  :)
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

Kaz

I have had more problems with this last batch of fusion than I have had previously. I thought it was just me as it has been stored in the shedio for quite a while. I am having real problems with the BHBs in rollers.
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

hollergrafik

Foster Fire regular for me, stays put on the mandrel but equally easy to get the beads off after.

Veebee

Thank you all very much! I have ordered some fosterfire for when I'm pressing or generally being thoroughly abusive to the beads in question. I'll keep the fusion for more normal beads  ;D

Ah Kaz, no it's not just you hun  ;)
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/


Shirl

I would like to get some Fosterfire as well, does anyone know of any suppliers that have it in stock?

Alison G

Bit late to the party but I have tried pretty much all of them, I like the Foster Fire but I think it's a pig to clean, it worries me as I have lung problems.

But at FO I found the best release ever! It's by Christina at Frit en Glas. You really have to get it hot to make the glass stick initially, but once you have it doesn't move. I have never had to use pliers to remove a bead and I don't soak them. I just clean outside now, it's much less dusty IMO because you can use a super thin layer.

I'm a convert!
NB. Do not touch hot rods of glass, it is stupid.

MadelineBunyan

Im not a presser, cant get on with the things, when I had one I did find fusion cracked.

I also find it cracks doing bhbs in rollers, but I think this is because of what Julie hb said about the bead release being cooler, one the last few beads that cracked, I've been noticing it more and more, the bead release definitely got too cold.

dusty Alison? are you not taking the beads off wet? even if they don't need soaking they should still be wet.

I will try some of Christina's bead release soon, but I wont be able to tell you what its like for pressing, cause I only have charmbox and I never use the bottom half anymore

GaysieMay

I always heat the mandrel right next to the bead hole at both sides before pressing and I do think this helps.
www.GaysieMay.etsy.com
www.facebook.com/gaysiemay

Alison G

Quote from: MadelineBunyan on April 22, 2011, 09:16:28 AM
Im not a presser, cant get on with the things, when I had one I did find fusion cracked.

I also find it cracks doing bhbs in rollers, but I think this is because of what Julie hb said about the bead release being cooler, one the last few beads that cracked, I've been noticing it more and more, the bead release definitely got too cold.

dusty Alison? are you not taking the beads off wet? even if they don't need soaking they should still be wet.

I will try some of Christina's bead release soon, but I wont be able to tell you what its like for pressing, cause I only have charmbox and I never use the bottom half anymore

I take them off inside a towel, I am really wary of the dust because I have chest problems, but no not wet.

Do you think I should?
NB. Do not touch hot rods of glass, it is stupid.

Shirl

YES.....do it wet. Then there is no dust, the dust is bad for you.

I dremmel mine underwater too.....get them nice and clean before using them.

MadelineBunyan

I have to say it did concern me a tad at FO, all these people happily pulling beads off dry, then buying kits and thinking its ok to do that when they're at home, making loads of beads.

I find that mine come off much easier, even just being dipped in water, also, I use the mandrel to clean out most of the bead release (which is easy to do wet) before I go near it with a diamond bit (diamond bits don't actually like bead release, particularly fusion, wears them out poor things)

drilling glass (which is essentially what you're doing when you are dremelling beads) is done wet for a number of reasons, cooling being one of them, and making the diamond bits last longer (presumably this is linked to the keeping it cool it thing). as well as this you've now not only got bead release dust flying around, but glass particles and anything that wears off the diamond bit.

sarah t

alison ..naughty naughty  ;D
soak em ,clean em ,ream em ..under water ....thats the beads and mandrels not you  :P ...and sal says dont tip the realease cleaning water down the sink ....but so much crap goes down my sink i think thats the least of my worries  ;D...famous last words ???

i did not think much to the christina release...thats not to say it aint good just did not work for me  ......maybe i did not get it hot enough ???......and it dries the same colour as the mandrel so i could not see it  :(........i had a bead stick on the mandrel which has not happened for yonks ......i would rather it went before i finished the bead ..not being able to get it off the mandrel is just not playing fair  :D......think i will stick to my forest fire ....

awrylemming

You clean them dry?!!  Scary lady, get them in a pot of water, clean them, drain off the water, scrape damp release into bin with kitchen roll, safer innit!