Best bead release for presses?

Started by Veebee, March 23, 2011, 02:06:13 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Veebee

Wot it said  :)

Those of you who use presses will know this situation, especially if it's a tricksy press that requires multiple pressing.... You make a bead, press a couple of times then the release cracks on you preventing further working. So what's the answer please? Which is the best release for using with presses?
I'v found blue Sludge to be much tougher than Fusion Plus, but Martin seems to have stopped selling it (it was only in the small pots but these seem to be fusion as well now?  :()

So do you have a favourite, and, where do you get it from?

Thanks!
;D
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

julieHB

Julie xx

                           My Webbie - My Flickr

JaySpangles

I use fusion - simply because I get it from Martin along with my other stuff, I just adjust the size of mandrel according to the press I am using.  (Generally for Zooziis I use 1.6, but 2mm is ok for Bavarian Beads and Beadpress.  Don't know about any others.

JKC

Do you let go of the mandrel when pressing?   I find that helps.

Veebee

Quote from: JKC on March 23, 2011, 02:14:28 PM
Do you let go of the mandrel when pressing?   I find that helps.

Yes, I do.  :)

Thank you guys

I have Fusion Plus Julie, we get along fine for regular beads but have a hate hate relationship with the press. I might have a go with a thinner mandrel though.

I've heard mention of Fosterfire elsewhere, anyone know if it's good for presses?
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

JKC

I just use Fusion, tried Fusion plus, doesn't work at all for me.

Blue Box Studio

Quote from: JKC on March 23, 2011, 02:56:50 PM
I just use Fusion, tried Fusion plus, doesn't work at all for me.

I didn't get on with it either.  I just assumed chipping the bead release on a press wa one of life's little challenges.
Sue
Website ~ Etsy ~ Blog ~ Flickr

mizgeorge

Fosterfire ;) Much tougher to break!!

♥♥Tan♥♥


Blue Box Studio

Heavy duty, smooth & tough, or regular?

[and yes, I am asking in the right thread!]  ::)
Sue
Website ~ Etsy ~ Blog ~ Flickr

♥♥Tan♥♥

 ;D ;D

I have used all of them and get pretty much the same results

Veebee

I just found that Bead shed listing with a search on google which came up with the FH supplier thread, how cool is that?!  ;D
Thank you all!
:-*
Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/

mizgeorge

I like smooth and tuff, but I agree, the results are just as good with all of them.

Shirley

I use FF regular. Wonderful stuff.
Val Cox Frit - Thai and Bali Silver 

Les

Quote from: mizgeorge on March 23, 2011, 03:33:33 PM
Fosterfire ;) Much tougher to break!!

And I am one rough mamma when I am beading ;D