Ian Pearson

Bob makes a lot of glass animals in soft and I have seen him make dragons, horses, etc.. from Borosilicate. Used to work for Pirelli or however the tyre company is called. Been making glass for years. teached at Plowdens and has great DVD out. Demoed at BSSG Symposiums. Photos of his work in GBUK Journal.

I have worked on sperate pieces and then joined them all up in flame. trick is flame control. Just made a parachutist and trick there was only heat the part of glass that you want to seal togtaher. can hold with fingers  if wholoe is not hot. Largets items I have made are about 24 inches long plus

Sorry for spelling but in a ruch

Ian

♥♥Tan♥♥

Thanks Ian, I shall give him a google ;)

fionaess

Quote from: Tan on February 10, 2011, 01:37:45 PM
Who is Bob Martin Pat?
Doesn't he make worming tablets for dogs?   ;D ;D ;D


If it's got a hole, it's a bead !

♥♥Tan♥♥

I have to admit thats what I thought :D

Brink Beads

Any ideas as to where you can get that DVD???
Sara

www.brinkbeads.co.uk

♥♥Tan♥♥


Brink Beads

Sara

www.brinkbeads.co.uk

Pat from Canvey

#52
Bob's contact info on the back cover of the DVD case is www.chixglass@tiscali.co.uk and you can see his horses at http://www.acclaimimages.com/_gallery/_pages/0028-0602-0606-1405.html