Main Menu

Iris gold yellow rods

Started by Shirl, February 08, 2011, 04:01:47 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Shirl

I bought this thinking it would be like the frit but it doesnt seem to want to play the same.

Does anyone have any of this colour, and what can I make with it? Any ideas will be welcome ;D

shaz

Eagerly watching this as ive bought the same and can only get poo from it  :'(
Sharon x

Kaz

Yep it's the yellow kind of poo!
Make the frit into stringer instead!
Kazx
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

♥♥Tan♥♥

Make little turds and sell them as bead poo ;D

helenfc


Shirl

 ;D ;D ;D

OK....so what do I do with my 5 fat rods of yellow poo?

Perhaps I can use them as chopsticks?

Someone must know of a good use for them?? :o :o

shaz

Only 5...ive got 7 and a half of the little sh..s left ;D
Sharon x

helenfc

Do they reduce? you could maybe put shiny dots on things with them?! x

Shirl

I dont think they reduce.

Perhaps we should have a competion to see who can get the best from this lovely glass ;D ;) ;D who know there might be an amazing discovery just waiting to be released.

I think I might experiment and choose some glass to go with it with my eyes closed.

Dragonfire Glass


squirsygirl

make an ivory olive shaped bead, melt the end of the iris gold ( about the size of a pea) get it good and hot.

Touch one side of the ivory olive, and spin yourself a 'thread' of the iris gold all over the olive.

Melt in very slowly and lightly, cool, then waft through a slightly reducing flame.

You should see some golden lines coming through, and can encase if you want.

I'll make an example tomorrow, and post a pikkie, if I get home from work in time.  IF!

Kirsty

♥♥Tan♥♥

One cool tip already.

Have you run a search on LE?

Shirl

Thanks Kirsty, I will try that later.

Tan, I havent run a search on LE as I always get sidetracked and start reading about other things....3 hours later I still havent got to what I first went to search for  :D ;D :D ;D

Hotglass28


I think I would turn it into frit too.  But I would heat and dunk it to make frit rather than crush it manually.

I have some of this colour too, can't remember what I did with it but I have a bundle tucked away. I'd be interested to see what people come up with this colour in rod form.

Good luck  ;)
www.facebook.com/pages/The-Owl-Goes-Hoot/567182803365298
www.etsy.com/uk/shop/TheOwlGoesHoot?ref=l2-shopheader-name

Trudi

I don't think that the 104 works anywhere near the same as the old 96 version! I know when I tried the 104 I couldn't get a thing out of it!