Trudi

Hi

the CIM Rose Quarts is opalino, and the effetre is clear, very pale

Pink Bubble Tutti Fruiti (2) by Glittering Prize - Trudi, on Flickr
the effetre rose quartz is the one on the far left - it is hard to photograph, but this gives you an idea! x

sundoorbeads

WOW Trudi that is a great colour reference!!! and I just grabbed the latest batch of my reg pink from effetre and they are all peachy toned on the ends :( the older ones I have from Reenie (flamekissed) are the last of the pinker toned ones :(
And yes silver will turn this one a more golden peach color!
Keep Flaming! Michelle

Dee Dee

Quote from: Mand on January 12, 2011, 12:54:32 PM
This is a shade I have struggled with too.   Hope you sort it. - Incidentally - love the shape of those heart beads - which press do you use?

Do you know, I can't remember - it's a long thin one without guides (so it needs a base) and it's got ridges on the back - maybe someone else who has one might know  (they don't call me Goldfish for nothing ;D )!

Dee Dee

Quote from: Helen G on January 12, 2011, 01:00:53 PM
looking at your beads (which are lovely btw) they all have SIS on them so I was wondering if the silver in that was fuming the pink glass to varying degrees? Have you tried making them without the SIS to rule this out??

That's a really good point Helen - I didn't think of that - I will try and see what happens! Thanks! ;D

Dee Dee

Thanks Trudi - those beads are lovely btw!  ;D

Trudi

Quote from: Dee Dee on January 12, 2011, 10:28:45 PM
Quote from: Mand on January 12, 2011, 12:54:32 PM
This is a shade I have struggled with too.   Hope you sort it. - Incidentally - love the shape of those heart beads - which press do you use?
I know the one, Mags did them, she only did a fewof them. She also did the multi tool!!!
I believe Lush has one (no surprise there). The Bavarian ones are very similar though!
Do you know, I can't remember - it's a long thin one without guides (so it needs a base) and it's got ridges on the back - maybe someone else who has one might know  (they don't call me Goldfish for nothing ;D )!

james M knox

Hi,

Dont know if this helps but I find I always have to strike the pinks to get them pink.
It also helps not to get them too hot and melty when shaping the bead.