Could someone just remind me ...

Started by Les, January 06, 2011, 09:01:21 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Les

Is it Laushca that doesn't get on with some glasses when used as encasing ?

sparrow

Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Les

Arse ! .... must have got the rod mixed up by mistake then ... at least I know it's not me .... damn nice beads they were too

Shirley

I use Lauscha transparent successfully when encasing effetre and some CIM. I've used it a fair bit with psyche and ekho as well with no problems. What were you making, Les?
Val Cox Frit - Thai and Bali Silver 

Les


Shirley

you should be fine as long as you haven't been heavy-handed with the frit. I always use Lauscha to encase by floral beads, so if they haven't cracked they probably won't, unless you used a strange combo.

Think you need to show us!
Val Cox Frit - Thai and Bali Silver 

Les