Double heated Luna!

Started by SuefromYorkshire, October 29, 2010, 06:15:16 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

SuefromYorkshire

I was trying to get the lovely purply/blue look under encasement like these, doesn't always work for me!
When I wasn't able to get the blues, I heated the whole bead up again (with encasement on) until bead was just about clear. Then after pressing (went all out of shape) thus cooling a few seconds I put it back into the cool part of the flame until I got some colour. Two centre beads.
Very strange but pretty, the colour seems to be above an pale centre  ??? Has anyone else done this with Luna, or have I accidently discovered something new?  :)

Trudi

Great beads - that's the way I work Luna too - as it's a striker!


Luna Nugget Duo by Glittering Prize - Trudi, on Flickr

I think if you search LE they have some tips on there!