Flyingcheesetoastie

I hope this is the right place for this, if not then please move me!

Anyway, I wanted to show the beads I was painting during Di's open day on Friday (8th October 2010) as I'm quite excited about what I tried.  Apologies it's a bit of a novel!

Basically I made some beads the night before using vetrofond (COE104), including my first lentil!  They were annealed overnight and left on the mandrels, to aid painting but also so I could try flame firing the enamels on.  I have many different types of enamel that I use in the studio, which all fire at different temperatures, can be mixed or not and also do different things when over fired, mixed with things outside the range etc.  So when I started making the enamel kits, the easiest thing was to use the same range so it was mixable and also fired at the same temperatures.  However the ones in the kits fire at between 620 - 720c which is too high for a standard anneal of a 104 bead, but in theory could be garaged and then flame fired.

Here are the results -



So, 4 beads, all a bit different.  The first one was a white base, painted with blues and a yellow sun, the blackness has occured because I tried a bit of low fire transparent enamel in the washes I was using, obviously this has burnt out due to the high temperature of the torch, but the other blue was fine.  The second was a black base with white enamel painted on and scratched away, quite a boring design but it shows another way of working with the enamels and also how they retain the crispness of the scratched line even when torched.  The third was a two tone blob in white and clear, which I painted mostly with the high fire but a little of a low fire bottle green, which has overfired to a blueish tint.  I like that you can see the design through the clear and this has loads of potential I think.  The last one was another white base that I entirely painted with black, torched and then stuck die cut stickers on once it was cool.  I then sandblasted it, which has given the crisp design and there's nothing to stop you taking this back up and encasing with clear or working further.

Anyway, I hope that gets the braincells firing as much as mine or at least explains what I was up to in my little corner on Friday!

Rachel x

GlassBeadArt

The ribbed beads look fantastic!
I have the small round ribbed roller and am not quite happy yet with my results, the ends of the beads are not perfect. Next torch time, I will try rolling the rounds first in a size smaller to get perfect ends and then only in the ribbed cavity...

The disc beads look aamzing; wonderful colour combination!

I have Autumn Bloom to show:

pixiewillow

Its been so long since I came here!! really should stop being so busy and come and play more often  ::) :D

heres a few of my new beads from the last couple of days....
P1120009 by pixiewillowdesigns, on Flickr

P1110988 by pixiewillowdesigns, on Flickr

P1110983 by pixiewillowdesigns, on Flickr

P1110894 by pixiewillowdesigns, on Flickr

P1110815 by pixiewillowdesigns, on Flickr


okay I'll stop hogging now!
Lorna XX
www.pixiewillow.etsy.com
www.pixiewillowdesigns.com
A mans idea of multi tasking is breathing & blinking at the same time.

Les

I adore that re focal Lorna !

Well here's the one set I managed to finish before my propane ran out yesterday....


Fruddy

...which is always scary - ya never know if they're going to break or not, because they aren't annealed!

Here's the latest batch...

Thanks for looking!   ;D


MangoBeads

#680
Lorna simply stunningly gorgeous  :)

.. I got a few hours bead time at the weekend between having lovely Astrid to stay and Lori's wonderful visit on Monday . I was having severe withdrawl after being no where near a torch when Astrid was here  :D

so I had a brilliant time



pixiewillow

Crikey thank you everyone  ;D ;D ;D

OOoooooo Manda they are beautiful!!

Heres a few from my kiln this morning

P1120070 by pixiewillowdesigns, on Flickr
P1120047 by pixiewillowdesigns, on Flickr

P1120046 by pixiewillowdesigns, on Flickr

and sometimes I like to make simple beads too!........

P1120068 by pixiewillowdesigns, on Flickr

these are hand shaped (until my crystal trio press arrives  ;) ;)).......
P1120060 by pixiewillowdesigns, on Flickr
www.pixiewillow.etsy.com
www.pixiewillowdesigns.com
A mans idea of multi tasking is breathing & blinking at the same time.

Tills

OK please be gentle... in fact I am having great difficulty getting up the nerve to post, given such beautiful beads this week, anyway I have been practicing encasing today, after "borrowing" some patience from Manda yesterday (Mango Beads) this is what I managed-  ;D










Secretly pleased as up until now I could not seem to master this!

helenfc

I have been making skull murrini today :) bead was a bit of a rush job (shocking photo sorry) but i will have a proper go at it tomorrow!  ;D

DSCN0854 by helenfchalmers, on Flickr

DSCN0859 by helenfchalmers, on Flickr

Tills

This started off as a play with Murrini, not sure how it got to this though  ???



Not sure if I love it or hate it!  :D

Barbara

Oh wow, what a show this week! 
My bead was made with Kalypso over Moretti 261 Angel pink:


Trudi

Some beautiful beads on here!

Gail - fab job on the encasing, it's such a relief when you get the hang of it!
Lorna - who needs a crystal press????? They look fab to me!


2 of your 5 a Day (1) by Glittering Prize - Trudi, on Flickr

Josephine

Pretty pendant Barbara.
Love those beads Trudi, such a pretty green.
I'm busy making for Big Bead. Here are some hearts I've done with my new Bavarian Beads heart press. (Sorry about the blue tac)











pixiewillow

Absolutely gorgeous!! I so wish I could work that silver glass..... sighhhhhh  ::)

Oh well, I can do brights!!  ;D

These are deep red (preparing for the C word!) but the photo turned them pink ugghhh  :-\



P1120086 by pixiewillowdesigns, on Flickr


And these are not my best beads in fact they are quite pants lol, I was just messing!!


P1120097 by pixiewillowdesigns, on Flickr
www.pixiewillow.etsy.com
www.pixiewillowdesigns.com
A mans idea of multi tasking is breathing & blinking at the same time.

Katiequiggle

Wow some fabulous beads here, very gorgeous. 

I made my first 40mm lentil about 2 weeks ago now but only just photographed it last week.  I'm very pleased with it even though its quit a simple one.