Turquoise coloured silver glass

Started by princess pink, July 02, 2010, 01:42:19 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

princess pink

Can't remember what it's called but seen a silver glass that reduces to a shimmer turquoise. Possible by double helix. Any ideas?

beadysam


hollergrafik



princess pink

I have no idea, can u show me beadies with both?? Xx

Emma @ Tuffnell Glass

Elektra 2 is a double helix Transparent glass....could it be this?

turnedlight

Sorry, I haven't tried the tag stuff - v. expensive, it just rang a bell when you said turquoise!
I have some elektra, I did wonder if you meant that - I have never really got on with it though.
kathryn

princess pink

ok stealing kate sullivans reef bead pic (which i am a proud owner of the bead) it's the tiny turquoise raised poked dots glass that i'm after!


helenfc


beadysam

I can get Black Nebula to go that shade if I heavily reduce it....

Nikki


flaming beads

Hven';t used Gaia for a while...but do remeber sometimes getting it to do that!

Lush!



www.lushlampwork.etsy.com

chipperpottery

Hi I used Tag Taxco over Cim Mermaid for the 3 larger beads and the small spacers were Cim Mermaid, just love this color.

Rita

http://www.flickr.com/photos/51048389@N02/4732917192/

paintboxcrafts

Hi,
I vote for Electra 2. I have only used it once, but it fits the description you want.