White spots on beads went funny colours after etching...?

Started by helbels, May 09, 2010, 09:14:22 PM

Previous topic - Next topic

0 Members and 3 Guests are viewing this topic.

helbels

Hi there

I made some basic pink beads (transparent) on Saturday with some white dots on them - pretty standard stuff.  When I etched them, the bead release has made the edges of the white dots go a sort of rusty brown colour in some places, and no matter how hard I scrub the colour won't come off.

My bead release is at the stage where it's starting to look like Cola.  Do you think this is why?  Should I be replacing it?

Thanks
Helen x

Dragonfire Glass

Mine looks like cola but I haven't noticed it discolour any beads  ???

sarah t

i always clean my beads before etching .......or did you mean the etch fluid is like cola ?

Lush!

I'm assuming you mean etching fluid, not bead release? 

I don't think my etching fluid has ever affected the colour (in a bad way!) even when it gets a bit old and cola-looking.

Any chance of a pic?


www.lushlampwork.etsy.com

Dragonfire Glass

Sorry - bead release is bead release colour, etching fluid looks like cola  ;D