saffie

I have just bought 1 rod of dark aurora and 3 of reactive cloud and wondered if anyone had any helpful hints on them. I know to encase the dark aurora to get best results. I am going to play with them tonight but with them being so expensive and not much I dod not want to waste them!!!
Thank you in advance
Sam

saffie

oops sorry Bullseye in case anyone is wondering xx

Hotglass28


I haven't yet played with these new colours. I thought they are copper reactive colours.  So any thing with copper in it will get the cload reacting.

Bullseye have a page which tells you which are reactives, which contain copper, what colours might react with another ect.

Clear as mud?

Have fun playing, let us know how you get on.......please!?

Denise