Main Menu

Faux Boro question

Started by helbels, October 21, 2009, 10:13:50 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

helbels

Hiya

I have read that interesting Faux boro effects can be achieved by using Straw Yellow & Iris Gold together, and have a few questions:

Would you use a rod of each of the different colour glasses and mix them to give this effect, or do you need to use Straw Yellow glass with Iris gold FRIT?

Do you need to reduce or do anything else to achieve the effect?

Is it possible on a Hothead?

Thanks!

Helen.







Trudi

You can use straw yellow dipped in iris gold frit and do one of 2 things:

get a blob of straw yellow - and dip in in iris gold (i usually do this 2/3 times) then re-heat and twist and pull.

But to make to go further
dip the rod into the frit and pull into stringer, and then take a rod of straw yellow and add 3 lines of the "fritted" rod. Heat and twist.

I'm sure that there are other ways - but this might help you!

Mary

No reason why you can't use the rod if you have one, this technique was developed before the Reichenbach colours were readily available as rods. They used to just be frits or big huge bars for glass blowers.

Trudi

I guess it depends on the rods - ages ago I tried the 104 Iris Gold and I got nothing from it.

Perhaps I might try it again.

Mary

That's a point Trudi, I've not tried it with 104.

Shirley

It works brilliantly with a hothead, by the way. Try it over cobalt transparent for greenyblue patterns, and over rubino you can get lovely ambers with lilac shades. All good fun.

In the Val Cox frit book she uses the iris gold frit with silver foil or leaf too to get some great reactions. Can't remember the details but someone who has the book will no doubt know. :)
Val Cox Frit - Thai and Bali Silver 

theflyingbedstead

QuoteNo reason why you can't use the rod if you have one, this technique was developed before the Reichenbach colours were readily available as rods. They used to just be frits or big huge bars for glass blowers.

I had problems trying this technique with Iris Gold rod (104), and was advised to use the Iris Gold frit instead, which did work for me.  I had presumed that the Reichenbach frit that I ordered from Martin was 104...but I now wonder if I am using the 92CoE instead?  That would explain why the rod and frit that I have look very different in colour.
Charlotte x

Shirley

I think the frit is generally the 90 something COE. The rods I've seen are 104.
Val Cox Frit - Thai and Bali Silver 

Trudi

yep - the 104 rod is yellow - I know when I tried it (and it was a while ago now) I got nothing from it. Don't even know why they gave it the same name!!

dinah46

Quote from: Trudi on October 21, 2009, 12:52:17 PM
yep - the 104 rod is yellow - I know when I tried it (and it was a while ago now) I got nothing from it. Don't even know why they gave it the same name!!

Yep - I got the same blah yellow with the 104 rod - frit or 96?coe rod is the way to go

Redhotsal

Yes, the Reichenbach frit that Martin sells is definitely NOT 104 - I've done a compatibility check on it. I've got both coes to work and both frit and rods to work but the 96 (or whatever it is) gives a better result. That yellow rod that was being flogged a little while ago is certainly NOT Iris Gold - looks nothing like the original 104 rod, which was gold.

A hothead will do faux-bo really well but don't reduce it at all or it'll go murky grey.

I love fauxbo - can't resist a little inpromptu show'n'tell....Sorry to hi jack!






Mary


helenfc

wow sal, they are just divine!!im saving up to start and this sort of thread makes me think i should stop eating so i can save faster!!  ;D

Mand

OMG! Those colours are fantabulous!  How did you get those, what did you use? I wanna try. ;D :P

Redhotsal

it's just good old Effetre straw yellow and  Reichenbach iris gold. Honest.
And it's cheeeeaaaaapppp!  ;D