bubblefizz

Has anyone got any pics of DH Gaia ?

Carol

Have a search Angie, there's some in the "DH on a HH" thread, & also Mary has posted lots in various other threads :)
Carol

Billie

Yes, there'll be quite a bit in Show n Tell  :)

Les

#3




These two were made with DH Gaia... ivory and ASK Silver Cinamon...
The Gia started out as green.. then as it gets worked, produced the greeny blues...

Pam

Ohhhh Ilike that. I must admit I have tried to use Gaia but failed miserably and its so expensive. You have inspired me Les.

Mary

I just realised these aren't in the archives here. Apologies for those of you who have seen them! With silver cinnamon, on ivory, and on black.

bubblefizz

Mary i LOVE the 2nd one, how do you do that???
did you pull a stringer first?

Mary

Yes Angie, the 2nd and 3rd are both applied stringer, in the 3rd it's melted in.

bubblefizz

Did you add clear to the stinger or just used as is?
i LOVE the 3rd one too, thats the one i was looking for, thats why i bought the gaia  ;D

Mary

No, no clear at all, just straight Gaia. I love Gaia!