I have been asked to make a set of beads in creams and I am struggling with effetre dark and light ivory because they are so reactive. Does anyone know if CIM Butter Pecan and Ginger are like ivory and react with other glasses please?

Stacy

I have no idea about glass I am afriad but just thought I would mention that I thought you had a funny tummy after eating a wierd sandwhich!

Helen G

 ;D ;D ;D ;D ;D yes, I see what you mean....the title ha ha ha

Helen G

OK, I'm dim, just read info on Off Mandrel and says they are less reactive. Sorry everyone!

saffie

they are excellent for not reacting I love them for that reason!


TiaraHelen

I got a strong reaction from butter pecan mixed with triton dots - it went a sort of caramac brown and the triton webbed a bit, so don't bother with that combo for your ivory set! 
Helen x

Even after all this time, the sun never says to the earth "you owe me".

Vicki

how about porcelain? I think it's riechenbach

Shirley

Effetre silver pink is good. Doesn't react and is barely pink at all.
Val Cox Frit - Thai and Bali Silver 

Josephine

Vetro ivory is paler and doesn't react as much as the effetre.