Jolene

I don't know much about silver glass.......is there one out there that is CoE 104 and reduces or strikes to shades of shimmering purple?

ta, Jo x

theflyingbedstead

Hi Jo, Double Helix Psyche can be reduced to produce some lovely purple hues, as well as peacock blues/greens. I'll see if I can find photo of one of my beads so you can see...
Charlotte x


theflyingbedstead

Also, TAG Dalai Lama can be struck to purpley blues.  I have just bought a stick but haven't tried it yet so here's a link! http://www.taglass.com/104.html
Charlotte x

theflyingbedstead

Found a picture of some of my Kristina Logan inspired beads - the smalled bead has psyche plunged dots.
Charlotte x

Lush!

Oh! What amazing, beautiful, gorgeous beads!


www.lushlampwork.etsy.com

theflyingbedstead

Aww - thanks - that's cheered me up this Monday morning!  ;D
Charlotte x

Jolene

Lovely lovely lovely thanks Charlotte

Will you let me know how you go with the TAG please?

Jo x

theflyingbedstead

Thank you!  I will...I'll be playing again at the weekend.
Full time job does get in the way of using my kiln during the week.
Charlotte x

Trudi

this has whispers of DH pysche in



and the square foacal is also DH pysche



Red Hot Sal is the queen of the stuff!

theflyingbedstead

QuoteRed Hot Sal is the queen of the stuff!

Yes...and terra!
Charlotte x

theflyingbedstead

Gorgous beads too, by the way; you've got a great range of colours there Trudi!
Charlotte x

Trudi

thank you - but they don't always turn out like that!!  ;D

Mary

I know it sounds odd, but emerald green Gaia is lovely too! Put on black the transparent green disappears, and you only get the iridescence.
I get pinks from Triton too, like the heart.




Stacy