Main Menu

CIM Lapis

Started by Dee Dee, January 28, 2009, 12:32:19 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Dee Dee

Finally having a go with some CIM Lapis that I've had for ages.  It seems to lose it's shine when I am working on it - am I doing something wrong?

Steph X

Lush!

Erm, you're probably reducing it a bit.  Turn your oxy up ... if you can!




www.lushlampwork.etsy.com

Dee Dee

Ahh Julie, I am on a hothead, so can't help that at the mo - but will shortly have my new torch and oxycon, so will take that note on board.

Btw - you are up late my dear!


Steph x