6mm SLUMPING firing schedule (ARTISTA)

Started by handmadeheaven.biz, January 06, 2007, 04:59:50 PM

Previous topic - Next topic

0 Members and 3 Guests are viewing this topic.

handmadeheaven.biz

SLUMPING 6mm firing schedule ARTISTA

1. 175C/hr to 540C   0.10

2. AFAP or 9999C/hr to 700C   0.00

3. 100C/hr to 790C   0.00

4. AFAP or 9999C/hr to 560C   1.00

5. 66C/hr to 443C   0.00

6. 125C/hr to 393C   0.00

7. AFAP or 9999C/hr to 25C   0.00