now I know that you cant use most precious and semi precious stones in glass as the heat would just disintergrate them...

but wot about diamonds... would it kill them as well...

saffie

right melting point is 3550 C so thats not an issue but would it survive annealing etc Mmmmm....dunno, could be expensive to find out  ;D

littlegiggles

lol.... I know... but you know when my mind starts scheming....

sparrow

Interesting......I've got a diamond I could play with....would be a bit of a bummer if the bead then was c***and nobody wanted it, lol!
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Kaz

I'm reading this thinking either I'm mad or they are..... :-\
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

littlegiggles

no... its most definately me... mad as accused

sparrow

Same here.....when I was doing silversmithing, I bought a broken diamond ring in America, thinking I could fix it and sel it on....never did, though  :-\
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Juniper

I doubt the diamond would survive. A diamond is still a natural stone with impurities an flaws, that might react when heated. But it's your stone ;)

Paula

Jolene

#8
I have seen it done with opals by Bruce St.John Maher....will try to find a link

Modified to add http://www.gemcutter.com/maher.htm

Gorgeous bits of glass.....he also makes jaw dropping murrine

sparrow

OMG Jo, what did you do that for!!!!! My wallet can't take another hit!  ;D
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Juniper

That opal is actually synthetic fire opal. It works with boro if you use small pieces - so I've been told ::)
Paula

littlegiggles

fire opal in boro... or little bitta boro fused in soft glass

Chameleon

i put an opal in soft glass an it survived.

.. no you cant see it, it was a totally shockingly bad bead in design and a complete fugly. but the opal did survive

sparrow

Can I see it if I ask really really nicely??  ;D ;D ;D
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Chameleon

lol, as its you, if i can find it to take a pic of then i will post it