♥♥Tan♥♥

I stick with effetre black, its never failed me yet and I've bunged allsorts on it, I found the vetro black can have a bit of a haze sometimes, almost as if its trying to be a silver glass...........but without the colours ::)

saffie

Quote from: tanok on October 23, 2008, 03:22:11 PM
I stick with effetre black, its never failed me yet and I've bunged allsorts on it, I found the vetro black can have a bit of a haze sometimes, almost as if its trying to be a silver glass...........but without the colours ::)

I was deeply into Hades black and still love it but it is quite a stiff glass. I have rediscovered effetre black and love it! it is quite happy to have most things shoved on it!!!

Im a glassy babe

ok, that's great, thanks for the help! ;D

Will go back to effetre or maybe give hades a go. x x V

Shirley

I love Hades, but you have to watch it because it can do fun things with other glass, especially silver glass. It really is a proper black, though. One of my favourites. :)
Val Cox Frit - Thai and Bali Silver 

Im a glassy babe

Thanks Shirley.  I suppose a lot of experimentation is in order.  Oh no, means more time beading. ;)