Odd and No-Lot - ??????????????

Started by sublimekate, September 09, 2008, 11:41:42 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

sublimekate

Quote from: glassworks on September 09, 2008, 03:25:14 PM
i'll make some paddles of these colours and also some of the odd and no-lot vetro's we've got and see if anything tickles ya fancy!....
;D ;)


Pinched this quote from another thread, this crops up every now and then, and I don't know what it means???

Can someone enlighten me pretty please.

kate x

Jolene

#1
Odd lots are colours of glass that have come out not as intended (sometimes with spectacular results) or are limited edition. Effetre have some which are now highly sought after as they are in short supply - Vetrofond produce a range of odd lots and CiM call their odd lots "Uniques" but I have never seen any CiM odd lots in real life. Odd lots tend to have a batch number witch is similar to the standard colour that they resemble but with an additional letter or number to identify that they are "odd".

The "no lots" have turned up recently since Quinton visited the Vetrofond factory, the colours don't even have names or batch numbers - I am not sure of the full story there ;D

glassworks

LOL..

the no-lots are literally glass i pulled from vetrofond's stock room myself, and they are colours or batches which were never made in quantity enough to sell.. these tend to be experimental batches, or the remains of glass made as a one off for a special order..

sublimekate