How do you get the nice swirly glass all wooshing around pattern?

Started by turquoise, September 01, 2008, 10:03:17 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

turquoise

Hi
I had a go at this the other day and the bead looked dire.

How do you do it so the colours all mix up along side each other?
Vic


www.morellobeads.co.uk

grandmabead

Well, i'm not sure what you mean exactly but are you talking about gravity beads???Got a pic as an example? For gravity beads just get them real hot and let them droop (which stretches the dots/stringers) then sort of wrap them back onto the mandrel and then shape. Sounds like i know what i'm doin don't it? LOL

Here's a pic of gravity beads i made - it's the one in the middle and on the right. A bit crap but it might be what you mean. Ignore the fugly on the left......i was trying out new things.


turquoise

You have got it spot on there duckie. Mine came out totally poo.

I will give it a whirl after lunch.
Thank you. ::) ::)


www.morellobeads.co.uk

Vicki

you can rake the colours around too, just make sure the bit you want to swoosh is nice & glowey & off you go ;D