Main Menu

clear frit on Dark ivory

Started by beads-on-toast, June 11, 2008, 11:22:37 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

beads-on-toast

DOES NOT WORK

unless you want a dirty grey look...shall post a pic tomorrow - just wanted to let ya know

greenbeadenvy

Yep clear on drk ivory is pants :D been there....got dissapointed :(. My very faves are clear over any of the ask colours, esp tirbal turq or berry creamy...yummy ;D
Emma xx

flowerjasper

oooh got some tribal tourquoise will give it a go!  ;)

Les

ooo.... i got some clear frit knocking about.... must give that a go :)

Thanks for sharing Anna... :)

xx

Kaz

Emma
Which clear frit do you mean over the ASK - I seem to have a couple of different ones? Would like to try this.
Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

greenbeadenvy

Crystal clear. here's a picture.
http://www.beadenvy.co.uk/Photos/Bead%20Sets/pages/BS006.htm
It makes a kind of lizzard/snake effect....cool ;D
Emma xx

Kaz

That is cool - I'll have a play later on. Thanks  :)
Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Mary

According to Val Cox a lot of the furnace frits have lead in, which is why we can use them with other coe's, but lead reacts with ivory. If you can get 104 clear frit you'd probably be OK. Sorry, font of useless information me!

Les

And we love you for it too Mary !!!!!!!!!!!!!!!!!!!!!!!!

;D ;D ;D

xxxxxxxxxxxxxxxxxxxxxxxxxxxx

beadysam

I love clear frit over copper green - then etched, yum! ;D

beads-on-toast

Quote from: beadysam on June 12, 2008, 12:45:32 PM
I love clear frit over copper green - then etched, yum! ;D

you cheeky minx!!! i shall have to try this combo now - oh how you tease us so