Can anyone help please?

I've been asked for black and white beads with silver - but the silver wire and the white make a mucky brown mess.  I think this is happening on both Effetre white and CIM Peace. 



I tried putting a clear band round the centre and wrapping the wire round that but it was just a mess.


Any better ideas?


www.lushlampwork.etsy.com

beadysam

Sorry, I'm no help but I just wanted to say the Anise does the same, it turns a yellow colour.  Good luck in finding a solution.  You could maybe try Reichenbach rods?  I don't have any white although I have plenty of black - maybe Martin can help?  Mary our resident alchemist may have a solution or suggestion for you.  Possibly a lauscha colour...?

garishglobes

I'm not going to be helpful with an alternative white either, but could you just put silver on the black half?

beads-on-toast

i love the reaction - looks like a choco coffee combo - but yes it is annoying, i have never been able to stop it

Billie

I think you'll have to use the silver on the black.  I think even if using the wire like stringer and applying single dots you'll still get the brown around the dot.

Lush!

Quote from: beads-on-toast on June 09, 2008, 02:00:02 PM
i love the reaction - looks like a choco coffee combo - but yes it is annoying, i have never been able to stop it

Well, when I'm asked for choco coffee combo beads I'll be sorted  ;)

;D ;D


www.lushlampwork.etsy.com

LesleyMac

Or you could encase the white maybe?
Lesley
Everyone is gifted, its just that some leave the wrapping on longer than others
(Richard Wilkins)


My Etsy http://www.etsy.com/shop.php?user_id=5469196

TiaraHelen


Would it work if you put a tiny blob of clear on the white and a dot of silver on top?
Helen x

Even after all this time, the sun never says to the earth "you owe me".

TiaraHelen

I just saw on RedHotSal's website front page, lots of white beadies with silver and NO BROWN stain.  What's your secret, Sal?
Helen x

Even after all this time, the sun never says to the earth "you owe me".

garishglobes

I'm just wondering.. did Q once say the Vetro white was nicely unreactive? Or even the odd cotton?

Lush!

Quote from: TiaraHelen on June 09, 2008, 06:53:59 PM
I just saw on RedHotSal's website front page, lots of white beadies with silver and NO BROWN stain.  What's your secret, Sal?

I think they may be ivory?  ::)

But I got rather distracted by those absolutely stunning "kimono" tubes  :o :o


www.lushlampwork.etsy.com

Kaz

Er wowowowowowow! She kept those a bit quiet, didn't she - wish I could afford the whole set - they are stunning! :o
Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

TiaraHelen

Quote from: Lush! on June 10, 2008, 10:12:13 AM
But I got rather distracted by those absolutely stunning "kimono" tubes  :o :o
Me too, they are fabulous...
Helen x