Main Menu

triton

Started by flowerjasper, May 30, 2008, 11:09:47 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

flowerjasper

oops i seem to have brought some triton rods from martins ebay shop   ::)
deary me,
anyone got any tips?
am on a hot head so a reducing glass should be ok  :)
sandy x

think i have tourettes of the fingers, they just cant help themselves   ... ;)

Sulis (Hazel)

LOL Sandy - I know that feeling!

Sorry I have no advice to offer.

I bought some too, but can't seem to do much with them yet. So far it's going quite a milky colour, or just goes mirror shiny. I want that lustre effect that's on the picture  ???

Have you tried anything at all yet?

Hazel x

flowerjasper

will give it a go when it arrives,
i too want it to look like the pic!   didnt do well with northstar double purple    :( :(

Kaz

I'm getting mirror shiny

Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Sulis (Hazel)

Hazel x

Caroline

it's buy far the easiest glass ever to reduce and i''ve been using it all week, you just waft it in a reducung flame and you get that lovely mirror shine

Billie

I can see your reflection Kaz  ;D ;D ;D

Vicki

I had some delivered this morning (thanks Martin) but I won't get to play for a few days, if anything groovy happens I will show you :)  Those are lovely lentils Kaz ;D

June

I was getting 'mirror' shiny last night, too.  I was also using M-166 at the same time and I can slightly see some colouring in it, not just pure silver.  I will have to post a piccie  ;D

Fiona - I have the same problem with Northstart double purple, I tried it again a few nights ago and there's a little blue around the edge near the mandrel, but the rest is pretty much 'poo' !!  I see you were after some psyche, I only have frit, but Martin will usually sell single rods if you get stuck.

flowerjasper

this is what i want to get!!
not really mirror shiny....

Clare Scott

#10
I`ve just put this together... triton & silvered ivory.



Depends on the effect you are going for - I reduce very little as I prefer the beautiful purples and greens rather than creamier colours..... I found it the easiest to use.

Clare x

flowerjasper

thats fab!
lovely colours not just mirror shiny!!
whisper your secret   ;)
sandy

June

Maybe I'm reducing a bit too much?  I'll have another go later or tomorrow.

turnedlight

With some of the DH glass, if you get the mirror finish then top with clear, you get the colours.. at least, I do it when I'm doing dots, topped with raised clear bumps..
I would love to know how long you are supposed to reduce, to get bright purple and pink colours.. after you heat it hot and let it cool, is it a quick waft or hold it in the reducing flame till it glows?
kathryn

♥♥Tan♥♥

Blimey, its a science in itself this silver glass malarkey :o