Filigrano ... mmmmm!

Started by Lush!, May 13, 2008, 10:23:03 AM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

Lush!

Well I've had a few rods of Effetre filigrano since I got my starter kit, but never really bothered to try them out, so what a nice surprise I had when I finally gave it a go!



I see Martin's got some in pink and violet - anybody tried them?

I'm also wondering how other people use this glass?  Its probably a bit pricey to use on its own like this!



www.lushlampwork.etsy.com

TiaraHelen

Very nice. I've been trying to get this effect with ordinary stringer, but it just melts in too much - maybe this is the answer...

Thanks for puttng the photo up,
Helen x

Even after all this time, the sun never says to the earth "you owe me".

Pam

Those are beautiful, so light and summery.

garishglobes

Very pretty! I love that light, wispy effect.
The filigrano cane looks great if you lay  several bits side by side and make a twisty - but while I just adore the twisty it makes (lovely fine lines) I've yet to use it successfully!! It just looks too thin on the bead...

Kaz

Julie - those are lovely  :) - I really like the filigrano rods and bought a batch from Howaco where they are a fair bit cheaper and have a wide range of colours. I also love the blue goldstone filigrano - the effect is very pretty too!
http://www.howacoglasssupplycompany.com/effetre_filigrana_rods.html
Kaz
She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!

Redhotsal

Cor Julie - they're gorgeous! Love the "wispy" effect!  ;D

Vicki

very pretty Julie, I used mine on its own as well :)

How did you get on with the blue gold stone one Kaz, mine was so shocky, I kept it on top of the kiln & it went all over the place even when it was at the point my asbestos hands couldn't actually hold it it still went all over the place :D

Carol

Well I've got quite a few rods of filigrano that haven't seen the light of day since I got them over a year ago - your lovely beads have inpired me to dust them off Julie :) (I did use some goldstone ages & ages ago, & it spat bits all over the place too  ::) :D )
Carol

♥♥Tan♥♥

Try a base of clear then a few wraps of this, same effect but a bit lighter on the old pocket!!

flowerjasper

filigrano petrol green,
wiggly snakes!! the left hand one is over light torquoise,

♥♥Tan♥♥

Absolutely chuffin gorgeous!!!

SueP

How spooky I tried using some of mine last weekend here are some little beadies of aqua filigrano over cim celadon just awaiting the batch anneal
;D :)


Lush!

Nice beadies Sandy & Sue  :)

Quote from: tanok on May 13, 2008, 03:27:28 PM
Try a base of clear then a few wraps of this, same effect but a bit lighter on the old pocket!!


Good idea Tan - I tried your method last night, and it worked just fine!   ;)



www.lushlampwork.etsy.com

June

Mmmmm, these beads are lovely.   ;D

♥♥Tan♥♥

Julie MMM MMMMM MMMMMMMMMMMMMMMMMMMm deeeevinneeee