Oiling cores?

Started by sparrow, April 03, 2008, 01:26:17 PM

Previous topic - Next topic

0 Members and 1 Guest are viewing this topic.

sparrow

As in, is anybody doing it? Is there a trick to it? I've tried (letting oil run though it, essentially), but it doesn't seem to make that much difference. I've been usng olive &vegetable oil so far, or do I need to get oil pressed out of midnight-blooming roses by the hands of blind, naked buddhist  (bead-hist?) monks from the outskirts of a small village near Ulaan-Baatar - and if so, is it on special offier anywhere?
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

garishglobes

I've never heard of doing this! How exciting, what does it do?! Is it particularly good for goddesses?

Lush!

What about clear nail varnish?



www.lushlampwork.etsy.com

sparrow

Have you tried that, Julie? Sounds interesting - that would mean my etched beads would get two nail varnish treatments!

Emma, the idea is you see less of the channel the hole makes through beads, particularly clear, light colours, I've been meaning to get to grips with it for ages....
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Lush!

I'm sure Ray Skene wrote something about this a while ago, and I think that's where I read the nail varnish tip - but no, I haven't tried it (have tried the part-etching thingy though, cool!)



www.lushlampwork.etsy.com

garishglobes

Aah, it all makes sense!  :) I have some bead polish which says it cleans holes. I've never got to grips with it, wonder if it does anything?

sparrow

For somebody who never wears nail varnish, I go through quite a bit......okay, it's on my shopping list......how on earth do you varnish inside a 1.6mm, up to 3" long hole......I guess I could pull thread through the varnish then through the bead.....*scuttles off to ponder*


Emma: don't know..........want to bring it on Saturday, and we'll explore?
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Lush!

Yeah, dip and pull thread or a pipe cleaner maybe?



www.lushlampwork.etsy.com

garishglobes

I don't wear nail varnish either, though our house is full of various shades of lurid pink, purple and glitter! Not sure they'd work for bead cores though. Actually, this bead cleaner suggests using a pipe cleaner too. Maybe that'd work for oil too?

sparrow

I'm planning to go into town tomorrow........must add pipe cleaners to my list!
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Fired Silver

Quote from: sparrow on April 03, 2008, 04:09:47 PM
I'm planning to go into town tomorrow........must add pipe cleaners to my list!

Sabine

Being a non-lampworker I have no idea what this thread is about!!  Just thought I'd mention though in case it's relevant - I use pipe cleaners for my metal clay work and I buy proper pipe cleaners, not the ones that you can get in crafty shops.  The proper ones have the metal bits in them and so don't disintergrate (sp??).  I use mine to thread through my metal beads when they're going into the tumbler to stop the shot getting trapped inside the beads - the cheapy ones just ended up as mush in the bottom of my tumbler!!  Don't know how they'd react to nail varnish!

Sorry if this isn't at all relevant!

Rebecca

sparrow

Thanks Rebecca, I'll make sure I buy proper pipe cleaners......if I can find them. Both craft shops and smokers' paraphernalia are in short supply in Sheffield city centre, but I'm sure I'll find some if I search hard enough :D
Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Fired Silver

I get mine at the cigarette counter at the supermarket - I have to ask for them though, they don't have them out on the shelf

Rebecca

sparrow

Sabine x

www.littlecastledesigns.co.uk www.facebook.com/littlecastledesigns Ring Top Tutorial

Lush!



www.lushlampwork.etsy.com