Main Menu

Recent posts

#71
Classified Ads / Re: Contents of glass studio
Last post by Nicknack - January 04, 2021, 11:51:35 PM
So sorry you're having to give up! I agree with the advice given, but, if it's fusing stuff, then Fused Glass Enthusiasts UK on FB would be a better group. There are often studios up for sale on there. Sometimes people ask if you'll split, can they have the moulds/glass/kiln etc., but you can decide if you want to, or if you'd rather it all went together. Best of luck!
Nick xx
#72
Classified Ads / Re: Contents of glass studio
Last post by Lynnybobs - January 04, 2021, 02:59:31 PM
Sorry to hear you are selling up but Moira has given some good advice there.
You could put some feelers out there on the destash Facebook page and see if there is any interest in the complete setup as a first step?
I guess money is tight for a lot of people just after Christmas so maybe smaller lots would sell better.
Good luck  :)
#73
Classified Ads / Re: Contents of glass studio
Last post by sandmor1 - January 03, 2021, 09:58:44 PM
Thank you Moira...that was a really comprehensive reply and is greatly appreciated.
Regards
Sandra.
#74
Classified Ads / Re: Contents of glass studio
Last post by Moira HFG - January 03, 2021, 10:32:41 AM
Sorry to hear you have to give up. As you say, it comes to us all eventually.

People used to sell on this site, it's still worth considering for the lurkers that look in from time to time, but most of the sales I see are on eBay and Facebook.

Ebay gets plenty of viewers, glass stuff seems to sell easily. You can either sell by auction to the highest bidder, or set a price.
On Facebook, search for the group 'EU Lampwork Destash'. A lot of glassy people use this to sell and buy, either setting a price or asking for bids up to a set date/time.

Things seem to go for around half to 3/4 their original value, depending on age and condition. Tools and moulds can go for more, if discontinued and/or hard to get. If unsure of the value, sell by auction and the market will decide!

Selling the whole lot is less work, but relies on finding someone who wants it all. There are many more people who would like just a kiln or specific tools.

Good luck with your sales!
#75
Classified Ads / Contents of glass studio
Last post by sandmor1 - January 02, 2021, 01:23:29 AM
Age comes to us all and sadly I can no longer do much in the way of glass fusing. I will have to sell it all. 2 kilns/glass/moulds and tools etc. But I don't know how I should go about it.
Should I sell it as a one off combined package or groups of like.
Should I advertise them on ebay auction or just on a for sale site.
I'm afraid I have never sold anything before and really don't know how to go about it.
Any advice would be appreciated.
Thanks
Sandra
#76
Looking For..... / Re: Peg type ends for rubber t...
Last post by BeeBeads - November 25, 2020, 01:03:57 PM
Thank you George.
#77
Looking For..... / Re: Peg type ends for rubber t...
Last post by mizgeorge - November 24, 2020, 12:33:35 PM
I make them in sterling. The biggest selection for base metals would probably be bijoux - https://www.bijouxbeads.co.uk/pvc-tubing/pvc-3mm
#78
Looking For..... / Peg type ends for rubber tube
Last post by BeeBeads - November 23, 2020, 01:40:43 PM
Can anyone tell me where I can find the peg-style type of closures for rubber tubing?  They're the ones that push into the tube ends and form a tight closure. 
Thank you!  :)
#79
COE 104 / Re: marbles
Last post by Dietmar - November 22, 2020, 02:02:57 PM
Marble making is fun.

If you need more practice, make after every day some "bench cleaner marbles". Get all leftovers from the bench and assort them roughly into color groups like blues, hot colors and greens. Heat the end of a stainless steel punty and stick the leftovers to the end. Heat the whole blob untill the air goes out and give it a nice twist with a second punty or a glass rod. Shape it with your marble mould and transfer to a clear glass punty to continue the shaping process on the other hemisphere.

A bubble free clear is a problem in 104. If you get a good batch try to keep the bubbles out while gathering it into a blob. Remove the scummy ends from freshly cleaned rods with your tweezers in the flame, before fusing them together. Avoid any folding operations and push the solid rods slowly into the maria or the gather between both ends. Let the gather cool untill it is solid and peel the outside if needed. Use this Gather as you would use a boro gather and keep it nice and warm while all operations.
#80
COE 104 / Re: green aventurine
Last post by Dietmar - November 22, 2020, 09:56:44 AM
There might be a tooo big difference in COE between the green and the other glass of the bead. I woulr like to see the broken surfaces to examine the way it broke. Glass tells you a lot about what went wrong, but you'll have to read it.

It might help to dilute that glass with a COE 104 glass. In a class I was told to use a transparent green (pea green) to mix it, but I choose the opaque version. The opacifier will break down but the lower viscosity might help better to make the COEs fit better.

If you do the stringer test, it shows how well the two glasses will fit in a combination. The test result should be straighter after mixing with the same amount of COE 104.