Difference between revisions of "Vetrofond"
From Fritipedia
Jump to navigationJump to searchLine 11: | Line 11: | ||
! Reactions | ! Reactions | ||
|- | |- | ||
− | | 1004 | + | |1004 |
− | | clear | + | |clear |
− | | colours appear lighter encased in clear | + | |colours appear lighter encased in clear |
| | | | ||
|- | |- | ||
− | | 1005 | + | |1005 |
− | | crystal clear | + | |crystal clear |
− | | good for encasing silver glass | + | |good for encasing silver glass |
| | | | ||
|- | |- | ||
− | | 1008 | + | |1008 |
− | | yellow | + | |yellow |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1012 | + | |1012 |
− | | light topaz | + | |light topaz |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1014 | + | |1014 |
− | | topaz | + | |topaz |
| | | | ||
− | | | + | |reacts with silver glass - reacts with silver to produce organic effects |
|- | |- | ||
− | | 1020 | + | |1020 |
− | | light grass green | + | |light grass green |
| | | | ||
− | | | + | |reacts with silver glass |
|- | |- | ||
− | | 1022 | + | |1022 |
− | | grass green | + | |grass green |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1024 | + | |1024 |
− | | dark grass green | + | |dark grass green |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1026 | + | |1026 |
− | | teal | + | |teal |
− | | | + | | |
| | | | ||
|- | |- | ||
− | | 1028 | + | |1028 |
− | | light emerald green | + | |light emerald green |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1030 | + | |1030 |
− | | emerald green | + | |emerald green |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1034 | + | |1034 |
− | | light aquamarine | + | |light aquamarine |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1036 | + | |1036 |
− | | aquamarine (aqua) | + | |aquamarine (aqua) |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1038 | + | |1038 |
− | | pale aquamarine (light aqua) | + | |pale aquamarine (light aqua) |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1040 | + | |1040 |
− | | light purple | + | |light purple |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1042 | + | |1042 |
− | | purple | + | |purple |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1044 | + | |1044 |
− | | dark purple | + | |dark purple |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1048 | + | |1048 |
− | | grey | + | |grey |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1052 | + | |1052 |
− | | light blue | + | |light blue |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1054 | + | |1054 |
− | | blue | + | |blue |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1058 | + | |1058 |
− | | intense blue | + | |intense blue |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1060 | + | |1060 |
− | | cobalt blue | + | |cobalt blue |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1064 | + | |1064 |
− | | black | + | |black |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1068 | + | |1068 |
− | | pink | + | |pink |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1069 | + | |1069 |
− | | electric yellow | + | |electric yellow |
− | | | + | |striking |
| | | | ||
|- | |- | ||
| 1072 | | 1072 | ||
− | | orange | + | |orange |
− | | | + | |striking |
| | | | ||
|- | |- | ||
− | | 1076 | + | |1076 |
− | | red | + | |red |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1080 | + | |1080 |
− | | pale lavender | + | |pale lavender |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1082 | + | |1082 |
− | | lavender blue (alexandrite) | + | |lavender blue (alexandrite) |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1084 | + | |1084 |
− | | light brown | + | |light brown |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1086 | + | |1086 |
− | | medium brown | + | |medium brown |
| | | | ||
| | | | ||
|- | |- | ||
− | | 1088 | + | |1088 |
− | | dark brown | + | |dark brown |
| | | | ||
| | | | ||
Line 371: | Line 371: | ||
|cosmic storm | |cosmic storm | ||
| | | | ||
− | | | + | |reacts with silver glass - bleeds in to ivory glass |
|- | |- | ||
|1802 | |1802 | ||
Line 395: | Line 395: | ||
|1806 | |1806 | ||
|smoke rings | |smoke rings | ||
− | | | + | |semi-transparent |
| | | | ||
|- | |- | ||
Line 415: | Line 415: | ||
|1810 | |1810 | ||
|lemongrass | |lemongrass | ||
− | | | + | |semi-transparent |
− | | | + | |reacts with iris gold frit |
|- | |- | ||
|1811 | |1811 | ||
|moon rock | |moon rock | ||
− | | | + | |striking |
− | | | + | |strikes from brick red to purplish coral |
|- | |- | ||
|1906 | |1906 | ||
Line 451: | Line 451: | ||
|Transparent amber (streaky amber)(antique amber) | |Transparent amber (streaky amber)(antique amber) | ||
| | | | ||
− | | | + | |reacts with silver glass - reacts with ivory |
|- | |- | ||
|1919 | |1919 | ||
|pale ivory | |pale ivory | ||
| | | | ||
− | | | + | |reacts with fine silver to produce organic effects |
|- | |- | ||
|1922 | |1922 |
Revision as of 16:15, 14 November 2008
Vetrofond glass is manufactured in Italy. Many stockists of Vetrofond glass rods use their own colour descriptions and stock numbers. The last 4 digits used by any stockist for their stock numbers will refer to the Vetrofond factory stock number.
Vetrofond colours and stock numbers
Transparent
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
1004 | clear | colours appear lighter encased in clear | |
1005 | crystal clear | good for encasing silver glass | |
1008 | yellow | ||
1012 | light topaz | ||
1014 | topaz | reacts with silver glass - reacts with silver to produce organic effects | |
1020 | light grass green | reacts with silver glass | |
1022 | grass green | ||
1024 | dark grass green | ||
1026 | teal | ||
1028 | light emerald green | ||
1030 | emerald green | ||
1034 | light aquamarine | ||
1036 | aquamarine (aqua) | ||
1038 | pale aquamarine (light aqua) | ||
1040 | light purple | ||
1042 | purple | ||
1044 | dark purple | ||
1048 | grey | ||
1052 | light blue | ||
1054 | blue | ||
1058 | intense blue | ||
1060 | cobalt blue | ||
1064 | black | ||
1068 | pink | ||
1069 | electric yellow | striking | |
1072 | orange | striking | |
1076 | red | ||
1080 | pale lavender | ||
1082 | lavender blue (alexandrite) | ||
1084 | light brown | ||
1086 | medium brown | ||
1088 | dark brown |
Opaque/pastels
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
1204 | white | ||
1206 | anice white | ||
1208 | silk white | ||
1212 | pea green | ||
1214 | nile green | ||
1216 | grass green | ||
1218 | dark grass green | ||
1220 | periwinkle | ||
1224 | light sky blue | ||
1228 | dark sky blue | ||
1232 | turquoise | ||
1236 | dark turquoise | ||
1240 | light lapis blue | ||
1242 | lapis blue | ||
1246 | cobalt blue | ||
1248 | light grey | ||
1250 | medium grey | ||
1255 | flower pink | ||
1262 | dark ivory | ||
1264 | light ivory | ||
1268 | pearl grey | ||
1272 | violet |
Specials
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
1408 | medium yellow | ||
1412 | dark lemon | ||
1420 | coral | ||
1424 | carrot red | ||
1428 | light red | ||
1432 | medium red | ||
1438 | red purple | ||
1444 | light brown | ||
448 | dark brown | ||
1456 | gold pink | ||
1460 | yellow ocher (wasabi) |
Odd lots
Stock Number | Colour | Properties | Reactions |
---|---|---|---|
1801 | cosmic storm | reacts with silver glass - bleeds in to ivory glass | |
1802 | apricot jam | ||
1803 | candy corn | ||
1804 | tomato soup | ||
1805 | orange dreamsicle | Reacts with [EDP] | |
1806 | smoke rings | semi-transparent | |
1807 | frog pond | ||
1808 | swamp moss | ||
1809 | jungle twilight | ||
1810 | lemongrass | semi-transparent | reacts with iris gold frit |
1811 | moon rock | striking | strikes from brick red to purplish coral |
1906 | chardonnay | ||
1909 | transparent green odd | ||
1910 | transparent yellow odd | ||
1911 | silk white (opal white) | ||
1912 | olive green pastel | ||
1917 | Transparent amber (streaky amber)(antique amber) | reacts with silver glass - reacts with ivory | |
1919 | pale ivory | reacts with fine silver to produce organic effects | |
1922 | transparent sage green | ||
1925 | transparent pale blue | ||
1926 | sea green (seafoam) | ||
1927 | ocean green | ||
1931 | river rock (brie)(avocado) | ||
1932 | fish pink | ||
1933 | pink no.3 | ||
1934 | pink flower | ||
1937 | arancio perfecto | ||
1938 | pale aqua streaky | ||
1939 | intense tangerine | ||
1943 | orange sherbert (free range salmon pink) | ||
1940 | italian marble | ||
1941 | pineapple yellow | ||
1942 | watermelon (poppy) | ||
1944 | tangerine | ||
1945 | new white (custard) | ||
1946 | sunshine 1947 yellow ice (lemon ice)(belgian lace) | ||
1948 | banana cream | ||
1949 | lemon meringue | ||
1951 | transparent candy apple red | ||
1952 | violet odd (purplicious) | ||
1954 | cool white (odd cotton) | ||
1955 | seashell swirl | ||
1957 | orange punch | ||
1958 | pyjama blue | ||
1960 | light pink | ||
1961 | carrot red | ||
1963 | green tepenade | ||
1964 | pale avocado | ||
1965 | olive green | ||
1966 | dark olive green | ||
1967 | quartz grey | ||
1968 | slate blue | ||
1969 | pearl grey | ||
1970 | transparent streaky sapphire | ||
1975 | midnight blue | ||
1976 | key lime green | ||
1977 | parrot green | ||
1978 | transparent crystal green | ||
1980 | light streaky brown | ||
1981 | streaky brown | ||
1982 | dark streaky brown | ||
1983 | pale ocean blue | ||
1984 | pale moss agate | ||
1985 | moss agate | ||
1986 | lichen | ||
1987 | dark lichen | ||
1988 | pale crystal green | ||
1989 | transparent odd topaz | ||
1990 | honey crunch | ||
1991 | marbled avocado | ||
1992 | banana | ||
1993 | sweet lime (red jasper) | ||
1994 | strawberry sweet (dark red jasper) |