Difference between revisions of "Reichenbach"
From Fritipedia
Jump to navigationJump to search (New page: Rechenback produce a limited range of colours in CoE 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the opaque Reichenback ...) |
|||
Line 1: | Line 1: | ||
− | [[ | + | [[Reichenback]] produce a limited range of colours in CoE 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the opaque Reichenback 104 glasses on a base bead of a very soft opaque colour (for example Effetre White) have a "bleed" effect rather than a crisp edge when melted down. |
Revision as of 18:23, 13 November 2008
Reichenback produce a limited range of colours in CoE 104. The opaque colours tend towards high colour saturation and so a little goes a long way. Dots made with the opaque Reichenback 104 glasses on a base bead of a very soft opaque colour (for example Effetre White) have a "bleed" effect rather than a crisp edge when melted down.